Optical constants of CDGM - QF (Light flint)
H-QF14
Wavelength:
µm
(0.360 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.48489196-0.00931778798λ^{2}+0.0204890803λ^{-2}+0.000525537026λ^{-4}-2.39700021\text{×}10^{-06}λ^{-6}+4.02659016\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 2.81e-07 1.63e-08 -1.07e-11 6.25e-07 4.08e-10 0.282 nd: 1.595512 Vd: 39.228024 glass_code: 596392 density: 2.62 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.8e-06 K-1 - temperature_range: 20 300 °C coefficient: 9.2e-06 K-1 dPgF: 0.0014 climatic_resistance: 1.0
References
CDGM Zemax catalog 2017-09 (obtained from http://www.cdgmgd.com)