Optical constants of CDGM - PK (Phosphate crown)
D-PK3-25
Wavelength:
µm
(0.300 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{0.513407653λ^2}{λ^2-0.00173535467}+\frac{0.923806373λ^2}{λ^2-95.3262202}+\frac{0.781224837λ^2}{λ^2-0.0118350221}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -3.49e-06 1.52e-08 -7.04e-11 4.13e-07 3.57e-10 0.131 nd: 1.523680 Vd: 70.274839 glass_code: 524703 density: 2.65 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 8.1e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 9.8e-06 K-1 dPgF: 0.0047 climatic_resistance: 2.0
Comments
anneal rate:25℃/h
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)
See also CDGM optical glass data sheets