Optical constants of CDGM - PK (Phosphate crown)
D-PK3
Wavelength:
µm
(0.300 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.29778839-0.00944743443λ^{2}+0.0107674711λ^{-2}-7.59126906\text{×}10^{-05}λ^{-4}+2.70221688\text{×}10^{-05}λ^{-6}-1.2965337\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -3.49e-06 1.52e-08 -7.04e-11 4.13e-07 3.57e-10 0.131 nd: 1.525006 Vd: 70.361017 glass_code: 525704 density: 2.65 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.1e-06 K-1 - temperature_range: 20 300 °C coefficient: 9.8e-06 K-1 dPgF: 0.005 climatic_resistance: 2.0
References
CDGM Zemax catalog 2017-09 (obtained from http://www.cdgmgd.com)