Optical constants of CDGM - LAK (Lanthanum crown)
D-LAK70
Wavelength:
µm
(0.280 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{0.616886534λ^2}{λ^2-0.000249888602}+\frac{1.11924765λ^2}{λ^2-0.0158113883}+\frac{1.29814839λ^2}{λ^2-102.017679}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 2.1e-06 1.31e-08 -3.75e-11 5.42e-07 6.96e-10 0.177 nd: 1.669100 Vd: 55.389689 glass_code: 669554 density: 3.35 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.3e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 9.1e-06 K-1 dPgF: -0.0066 climatic_resistance: 1.0
Comments
anneal rate:4℃/h
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)
See also CDGM optical glass data sheets