Optical constants of CDGM - LAK (Lanthanum crown)
D-LAK52
Wavelength:
µm
(0.280 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.04647517λ^2}{λ^2-0.0173536556}+\frac{0.889910862λ^2}{λ^2-0.00298398431}+\frac{1.23173612λ^2}{λ^2-87.1100488}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 1.8e-06 1.72e-08 -5.24e-11 4.52e-07 1.37e-10 0.229 nd: 1.730500 Vd: 53.944268 glass_code: 731539 density: 4.0 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 6.1e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 7.8e-06 K-1 dPgF: -0.0083 climatic_resistance: 1.0
Comments
anneal rate:4℃/h
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)
See also CDGM optical glass data sheets