Optical constants of CDGM - LAK (Lanthanum crown)
D-LAK5-25
Wavelength:
µm
(0.280 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{0.60236351λ^2}{λ^2-3.07499779\text{×}10^{-08}}+\frac{1.15823046λ^2}{λ^2-0.0158379352}+\frac{1.30267215λ^2}{λ^2-101.976296}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 1.76e-06 1.72e-08 -6.77e-11 3.92e-07 6.44e-10 0.23 nd: 1.676860 Vd: 54.805426 glass_code: 677548 density: 3.37 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.3e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 9.4e-06 K-1 dPgF: -0.0069 climatic_resistance: 1.0
Comments
anneal rate:25℃/h
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)
See also CDGM optical glass data sheets