Optical constants of CDGM - LAK (Lanthanum crown)
D-LAK5

Wavelength: µm
 (0.280 – 2.400)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula

$$n^2=2.76433988-0.0131613327λ^{2}+0.0182673276λ^{-2}+0.000301224328λ^{-4}+4.56200323\text{×}10^{-06}λ^{-6}-2.05087278\text{×}10^{-09}λ^{-8}$$

Conditions & Spec sheet

n_absolute: false
wavelength_vacuum: false
temperature: 20.0 °C
thermal_dispersion:
  - type: "Schott formula"
    coefficients: 1.76e-06 1.72e-08 -6.77e-11 3.92e-07 6.44e-10 0.23
nd: 1.677900
Vd: 54.896588
glass_code: 678549
density: 3.37 g/cm3
thermal_expansion:
  - temperature_range: -30 70 °C
    coefficient: 7.3e-06 K-1
  - temperature_range: 20 300 °C
    coefficient: 9.4e-06 K-1
dPgF: -0.0069
climatic_resistance: 1.0

References

CDGM Zemax catalog 2017-09 (obtained from http://www.cdgmgd.com)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

CDGM Glass Co., Ltd.

CDGM Glass Co., Ltd. is a leading optical glass supplier in China with a worldwile distribution network.