Optical constants of CDGM - LAF (Lanthanum flint)
D-LAF53-25
Wavelength:
µm
(0.290 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.32239317λ^2}{λ^2-0.00606224219}+\frac{0.646347208λ^2}{λ^2-0.0234824415}+\frac{1.17507569λ^2}{λ^2-87.8164211}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 7.67e-06 2.36e-08 -1.95e-10 6.35e-07 3.67e-10 0.208 nd: 1.742100 Vd: 49.246024 glass_code: 742493 density: 4.26 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 5.6e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 7.2e-06 K-1 dPgF: -0.009 climatic_resistance: 1.0
Comments
anneal rate:25℃/h
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)