Optical constants of CDGM - KF (Crownflint)
H-KF6
Wavelength:
µm
(0.340 – 2.400)
Derived optical constants
n
k
logX
logY
eV
Dispersion formula
$$n^2=2.26924681-0.0111135716λ^{2}+0.010955079λ^{-2}+0.000811179449λ^{-4}-7.07180723\text{×}10^{-05}λ^{-6}+4.69509667\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -5.94e-07 1.77e-08 -1.13e-10 5.53e-07 9.82e-10 0.212 nd: 1.517419 Vd: 52.189003 glass_code: 517522 density: 2.47 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7e-06 K-1 - temperature_range: 20 300 °C coefficient: 8.8e-06 K-1 dPgF: 0.0005 climatic_resistance: 1.0
References
CDGM Zemax catalog 2017-09 (obtained from http://www.cdgmgd.com)