Optical constants of CDGM - K (Crown)
H-K9LA
Wavelength:
µm
(0.290 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{0.684743072λ^2}{λ^2-0.00313539741}+\frac{0.586772376λ^2}{λ^2-0.014810133}+\frac{1.14804248λ^2}{λ^2-116.583792}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 9.03e-07 1.85e-08 -2.98e-11 4.55e-07 1e-10 0.182 nd: 1.516800 Vd: 64.198695 glass_code: 517642 glass_status: standard density: 2.51 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.2e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 8.8e-06 K-1 dPgF: -0.0013 climatic_resistance: 1.0
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)
See also CDGM optical glass data sheets