Dispersion formula
$$n^2=2.27196941-0.00991721869λ^{2}+0.0103697525λ^{-2}+0.000311903798λ^{-4}-2.64582145\text{×}10^{-05}λ^{-6}+1.64750848\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -1.13e-06 1.97e-08 -4.03e-11 4.17e-07 -1.86e-10 0.214 nd: 1.516797 Vd: 64.212351 glass_code: 517642 glass_status: standard density: 2.52 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.6e-06 K-1 - temperature_range: 20 300 °C coefficient: 9.5e-06 K-1 dPgF: -0.0023 climatic_resistance: 2.0
References
CDGM Zemax catalog 2017-09 (obtained from http://www.cdgmgd.com)
Data
INFO
BK7 optical glass
BK7 is a very popular crown glass. Most glass makers produce this glass under slightly different names.Analogs of BK7 glass produced by different makers
Maker | Glass |
---|---|
SCHOTT | N-BK7 |
OHARA | S-BSL7 |
HIKARI | J-BK7A |
CDGM | H-K9L |
HOYA | BSC7 |
SUMITA | K-BK7 |
LZOS | K8 |