Optical constants of CDGM - K (Crown)
D-K9-25
Wavelength:
µm
(0.290 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.08234297λ^2}{λ^2-107.907645}+\frac{0.548438846λ^2}{λ^2-0.002190929}+\frac{0.719999855λ^2}{λ^2-0.013407002}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 4.87e-06 1.55e-08 -1.35e-11 4.17e-07 5.2e-10 0.177 nd: 1.515770 Vd: 63.989637 glass_code: 516640 density: 2.41 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 6.3e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 7.8e-06 K-1 dPgF: -0.0029 climatic_resistance: 1.0
Comments
anneal rate:25℃/h
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)