Optical constants of CDGM - K (Crown)
D-K59-25
Wavelength:
µm
(0.302 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.16665743λ^2}{λ^2-0.00707953299}+\frac{0.105028598λ^2}{λ^2-0.0261090052}+\frac{0.990269002λ^2}{λ^2-98.6724455}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 5.85e-06 2.25e-08 -1.51e-10 3.09e-07 -8.98e-10 0.268 nd: 1.516980 Vd: 63.408500 glass_code: 517634 density: 2.41 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 6e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 8e-06 K-1 dPgF: -0.0029 climatic_resistance: 1.0
Comments
anneal rate:25℃/h
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)
See also CDGM optical glass data sheets