Dispersion formula
$$n^2-1=\frac{0.973027043λ^2}{λ^2-0.004919458}+\frac{0.077363216λ^2}{λ^2-0.01820094}+\frac{0.687944956λ^2}{λ^2-159.44609}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -2.24e-05 -5.6e-09 -9.96e-12 3.32e-07 4.01e-12 0.182 nd: 1.437800 Vd: 94.523389 glass_code: 438945 density: 3.52 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 1.43e-05 K-1 - temperature_range: 20 300 ℃ coefficient: 1.69e-05 K-1 dPgF: 0.0487 climatic_resistance: 1.0
Comments
anneal rate:4℃/h
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)