Optical constants of CDGM - FK (Fluor crown)
D-FK61

Wavelength: µm
 (0.280 – 2.400)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{0.872991432λ^2}{λ^2-0.00422111331}+\frac{0.756437828λ^2}{λ^2-151.201184}+\frac{0.344497102λ^2}{λ^2-0.0138938225}$$

Conditions & Spec sheet

n_absolute: false
wavelength_vacuum: false
temperature: 20.0 ℃
thermal_dispersion:
  - type: "Schott formula"
    coefficients: -2.45e-05 -2.09e-09 -6.72e-13 3.69e-07 2.37e-10 0.173
nd: 1.497000
Vd: 81.611615
glass_code: 497816
density: 3.9 g/cm3
thermal_expansion:
  - temperature_range: -30 70 ℃
    coefficient: 1.45e-05 K-1
  - temperature_range: 20 300 ℃
    coefficient: 1.7e-05 K-1
dPgF: 0.0322
climatic_resistance: 1.0

Comments

anneal rate:4℃/h

References

CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)
See also CDGM optical glass data sheets

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

CDGM Glass Co., Ltd.

CDGM Glass Co., Ltd. is a leading optical glass supplier in China with a worldwile distribution network.

External links


Glass

External links