Optical constants of CDGM - F (Flint)
F4GTI
Wavelength:
µm
(0.320 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{0.953714037λ^2}{λ^2-115.513417}+\frac{1.31399551λ^2}{λ^2-0.00931937546}+\frac{0.24063751λ^2}{λ^2-0.0452869078}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -2.9e-06 2.24e-08 -2.95e-11 9.73e-07 8.74e-10 0.246 nd: 1.620050 Vd: 36.430813 glass_code: 620364 density: 3.57 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 9.1e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 1.11e-05 K-1 dPgF: -0.0001 climatic_resistance: 1.0
Comments
i line glass
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)