Optical constants of CDGM - F (Flint)
F3
Wavelength:
µm
(0.320 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.54428229-0.00835307611λ^{2}+0.0228231808λ^{-2}+0.000670214922λ^{-4}+1.04294821\text{×}10^{-06}λ^{-6}+3.03297376\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 3.64e-07 1.78e-08 -2.72e-11 9.68e-07 1.31e-09 0.235 nd: 1.616592 Vd: 36.627394 glass_code: 617366 density: 3.57 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.5e-06 K-1 - temperature_range: 20 300 °C coefficient: 1e-05 K-1 dPgF: -0.0026
References
CDGM Zemax catalog 2017-09 (obtained from http://www.cdgmgd.com)