Optical constants of CDGM - BAF (Barium flint)
H-BAF3
Wavelength:
µm
(0.330 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.45168402-0.00862082666λ^{2}+0.0153497797λ^{-2}+0.000182555027λ^{-4}+1.41449954\text{×}10^{-05}λ^{-6}-1.68159962\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 3.07e-06 1.1e-08 8.58e-11 5.69e-07 1.29e-09 0.205 nd: 1.579568 Vd: 53.737216 glass_code: 580537 density: 3.14 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6.7e-06 K-1 - temperature_range: 20 300 °C coefficient: 8.4e-06 K-1 dPgF: -0.0009 climatic_resistance: 1.0
References
CDGM Zemax catalog 2017-09 (obtained from http://www.cdgmgd.com)