Optical constants of BARBERINI - Normal Crown
D0391: UV-W 76

Wavelength: µm
 (0.43583 – 0.65627)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Comments

20 °C
Normal Crown Glass (Uni/Bifocal); Colour: clear; Application: UV-absorbing glass for corrective lenses also suitable for technical applications

References

Barberini D0391 glass specifications, 2010-06

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

Barberini GmbH

Barberini GmbH is a German branch of Barberini S.p.A., the Italian company specializing in ophthalmic materials. Barberini GmbH has been formed after Barberini acquired the ophthalmic division of Schott AG in 2010.