Optical constants of GLASS
Soda-lime glass - Green
Wavelength:
µm
(0.32 – 4.6)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n=1.5130-0.003169λ^{2}+0.003962λ^{-2}$$Comments
Green soda lime silica window glass
References
M. Rubin. Optical properties of soda lime silica glasses, Sol. Energy Mater. 12, 275-288 (1985)
Data
INFO
Soda lime glass
Soda-lime glass is the most prevalent type of glass, used for windowpanes and glass containers. Soda-lime glass accounts for about 90% of manufactured glass.Other name
- Soda lime silica glass