Optical constants of Ag (Silver)
Johnson and Christy 1972: n,k 0.188-1.94 µm
Wavelength:
µm
(0.1879 – 1.9370)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Comments
Room temperature
References
P. B. Johnson and R. W. Christy. Optical constants of the noble metals, Phys. Rev. B 6, 4370-4379 (1972)