RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of C6H3Cl3 (Trichlorobenzene, TCB)
Myers et al. 2018: 1,2,4-TCB; n,k 1.28–25.0 µm

Wavelength: µm
 (1.28244E+00–2.50203E+01)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

temperature: 299

Notes

1,2,4-Trichlorobenzene, 26 °C

References

T. L. Myers, R. G. Tonkyn, T. O. Danby, M. S. Taubman, B. E. Bernacki, J. C. Birnbaum, S. W. Sharpe, T. J. Johnson. Accurate measurement of the optical constants n and k for a series of 57 inorganic and organic liquids for optical modeling and detection. Appl. Spectrosc. 72, 535-550 (2018) (see Supplemental Material for numerical data)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Trichlorobenzene

Trichlorobenzene (C6H3Cl3) is a chlorinated derivative of benzene that exists in three isomeric forms: 1,2,3-trichlorobenzene, 1,2,4-trichlorobenzene, and 1,3,5-trichlorobenzene. These colorless liquids are relatively insoluble in water but soluble in organic solvents. Trichlorobenzenes are utilized for various purposes, including as a solvent for a range of materials, an intermediate in chemical synthesis, and a dielectric fluid in transformers. Due to their persistent nature and potential environmental concerns, their use has become more regulated in many jurisdictions. When investigating trichlorobenzene's optical properties, it's important to note which isomer is under consideration as properties can vary. Handling should be performed with caution, ensuring adequate ventilation and avoiding prolonged exposure.

Isomers: 1,2,3-Trichlorobenzene; 1,2,4-Trichlorobenzene; 1,3,5-Trichlorobenzene.

Other names and variations

  • C6H3Cl3
  • TCB
  • 1,2,3-Trichlorobenzene
  • 1,2,4-Trichlorobenzene
  • 1,3,5-Trichlorobenzene

Links