Optical constants of C7H8 (Toluene)
Moutzouris et al. 2013: n 0.450–1.55 µm
Complex refractive index (n+ik)
Derived optical constants
Dispersion formula
$$n^2=2.161659124+0.000495188λ^{2}+0.02138179λ^{-2}+0.000058838λ^{-4}+0.000087632λ^{-6}$$Conditions
temperature: 300
Comments
300 K (27 °C).
References
K. Moutzouris, M. Papamichael, S. C. Betsis, I. Stavrakas, G. Hloupis, D. Triantis. Refractive, dispersive and thermo-optic properties of twelve organic solvents in the visible and near-infrared. Appl. Phys. B 116, 617-622 (2013)
Data
Additional information
About Toluene
Toluene (C7H8) is a clear, colorless liquid with a distinctive, pungent odor reminiscent of paint thinners. It is a naturally occurring hydrocarbon, found at low concentrations in crude oil and is a major component of gasoline. Toluene is widely used as an industrial solvent for paints, coatings, adhesives, and other applications. Furthermore, it serves as an important precursor in the synthesis of a variety of chemicals, especially benzene, xylenes, and a range of polymers and resins. Due to its refractive qualities, it can be of interest in optical studies. While it has various industrial and chemical applications, toluene is also known to have neurotoxic effects and can be harmful if inhaled in large quantities. Proper care should be taken when working with this compound.
Other names and variations
- C7H8
- Methylbenzene
- Phenylmethane
- Toluol
- Anisen
Links