Optical constants of C28H31ClN2O3 (Rhodamine 6G)
Seçkin et al. 2023: n,k 0.193–1.69 µm

Wavelength: µm
 (0.1930–1.6900)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

substrate: Si

Comments

Rhodamine 6G thin film spin-coated on Si substrate

References

S. Seçkin, P. Singh, A. Jaiswal, T. A. F. König. Super-radiant SERS enhancement by plasmonic particle gratings. ACS Appl. Mater. Interfaces 15, 43124–43134 (2023) (Numerical data kindly provided by Dr. Tobias A. F. König)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]