RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of C3H7OH (Propanol)
Sani and Dell'Oro 2016: iso-propanol; Dispersion formula; n,k 0.185–2.8 µm

Wavelength: µm
 (0.185–2.8)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{0.0107λ^2}{λ^2-8.88}+\frac{0.8702λ^2}{λ^2-0.01036}$$

Comments

Room temperature

References

E. Sani and A. Dell'Oro. Spectral optical constants of ethanol and isopropanol from ultraviolet to far infrared. Opt. Mater. 60, 137-141 (2016)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Propanol

Propanol (C3H8O), also commonly referred to as propyl alcohol, comes in two isomeric forms: n-propanol (or 1-propanol) and isopropanol (or 2-propanol). These alcohols are clear, colorless liquids that are miscible with water and have a characteristic alcoholic odor. Both forms of propanol are used as solvents in the pharmaceutical, cosmetic, and chemical industries. n-Propanol is often employed in the manufacture of antiseptics, detergents, and disinfectants, whereas isopropanol, popularly known as rubbing alcohol, is used for its antiseptic properties and as a cleaning agent. In optics, the refractive properties of propanol can be explored when it's used as a medium or in conjunction with other materials to modify light behavior.

Chemical formula (1-Propanol): CH3CH2CH2OH

Chemical formula (Isopropanol): (CH3)2CHOH

Other names and variations

  • C3H8O
  • 1-Propanol
  • Isopropanol
  • Propan-1-ol
  • n-Propyl alcohol
  • n-Propanol
  • n-PrOH
  • Ethylcarbinol
  • 1-Hydroxypropane
  • Propanol
  • Propionic alcohol
  • Propionyl alcohol
  • Propionylol
  • Propyl alcohol
  • Propylic alcohol
  • Propylol
  • Isopropyl alcohol
  • 2-Propanol
  • Propan-2-ol
  • Isopropyl alcohol
  • Rubbing alcohol
  • Sec-propyl alcohol
  • s-Propanol
  • iPrOH
  • IPA

Links