Optical constants of Propanee soot
Dalzell and Sarofim 1969: n,k 0.4358–10 µm

Wavelength: µm
 (0.4358–10.0)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Room temperature

References

W. H. Dalzell and A. F. Sarofim. Optical constants of soot and their application to heat-flux calculations. J. Heat Transfer 91, 100-104 (1969)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Soot