Optical constants of (C2H4O)n (Polyvinyl alcohol, PVA)
Bodurov et al. 2016: n 0.405–0.635 µm

Wavelength: µm
 (0.405–0.635)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{1.1490λ^2}{λ^2-0.1234783^2}$$

Conditions

temperature: 297
film_thickness: 1.0E-5
substrate: glass

Notes

10-μm film on glass substrate. 24 °C.

References

I. Bodurov, I. Vlaeva, A. Viraneva, T. Yovcheva, S. Sainov. Modified design of a laser refractometer. Nanosci. Nanotechnol. 16, 31-33 (2016)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Polyvinyl alcohol

Polyvinyl alcohol (PVA, (C2H4O)n) is a water-soluble synthetic polymer that exhibits excellent film forming, emulsifying, and adhesive properties. Due to its hydrophilic nature and high biocompatibility, it is frequently employed in a variety of biomedical applications, including drug delivery systems and wound care products. In the realm of optics, PVA is commonly used as a base material for hydrogel contact lenses due to its comfort and permeability to oxygen. It is also utilized in the creation of polarizing films for LCDs. PVA's unique structural characteristics, which include a mix of both crystalline and amorphous regions, can influence its optical properties. This polymer is also known for its barrier properties against gases, making it useful in packaging. One of the interesting attributes of PVA is its ability to form hydrogels when treated appropriately, expanding its range of potential applications. While it possesses many advantageous qualities, it is important to note that PVA is sensitive to moisture, which can alter its physical properties.

Other names and variations

  • (C2H4O)n
  • PVA
  • Poly(vinyl alcohol)
  • PVOH
  • PVAl
  • Kuraray Poval
  • Mowiol
  • Celvol
  • Polyviol
  • Elvanol

Links