Optical constants of (C3H4O2)n (Polylactic acid, PLA)
Bodurov et al. 2016: PDLA; n 0.405–0.635 µm

Wavelength: µm
 (0.405–0.635)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{0.9809λ^2}{λ^2-0.2123719^2}$$

Conditions

temperature: 297
film_thickness: 4.5E-5
substrate: glass

Comments

PDLA. 45-μm film on glass substrate. 24 °C.

References

I. Bodurov, I. Vlaeva, A. Viraneva, T. Yovcheva, S. Sainov. Modified design of a laser refractometer. Nanosci. Nanotechnol. 16, 31-33 (2016)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Polylactic acid

Polylactic acid (PLA, (C3H4O2)n) is a biodegradable and bioactive thermoplastic derived from renewable resources like corn starch or sugarcane. It has captured significant attention due to its compostability under industrial conditions, positioning it as an eco-friendly alternative to petroleum-based plastics. PLA is utilized in a multitude of applications ranging from food packaging to biomedicine, such as drug delivery systems and surgical implants. In the realm of optics, PLA is typically transparent, with a refractive index that can be influenced by factors like crystallinity and processing methods. Though its mechanical strength is comparable to that of polystyrene, PLA has a lower melting temperature, which can limit its use in certain high-temperature applications. Nevertheless, due to its biocompatibility and environmentally friendly nature, polylactic acid continues to be a material of interest for both research and commercial purposes.

Other names and variations

  • (C3H4O2)n
  • Poly(lactic acid)
  • Polylactide
  • PLA
  • Polylactide
  • PDLA
  • Poly-D-lactide
  • PLLA
  • Poly-L-lactide
  • PDLLA
  • Poly-DL-lactide

Links