Optical constants of (C5H8O2)n (Poly(methyl methacrylate), PMMA)
Szczurowski 2013: n 0.405–1.08 µm
Complex refractive index (n+ik)
Derived optical constants
Dispersion formula
$$n^2-1=\frac{0.99654λ^2}{λ^2-0.00787}+\frac{0.18964λ^2}{λ^2-0.02191}+\frac{0.00411λ^2}{λ^2-3.85727}$$Conditions
temperature: 296
Notes
23 °C. PMMA synthesized in Marie-Curie University in Lublin, Poland
References
Marcin Szczurowski. Private communications (2013) [[original data](https://refractiveindex.info/download/data/2013/Szczurowski - n_PMMA_raw.png)].
Data
Additional information
About Poly(methyl methacrylate)
Pentanol (Amyl alcohol, C5H12O) is an organic compound that belongs to the alcohol family. There are several isomers of pentanol, with the common name "amyl alcohol" often referring to a mixture of these isomers. Predominantly, it's used as a solvent and an intermediate in the production of other chemicals. In its pure form, pentanol has a characteristic alcoholic odor and is slightly viscous compared to lower alcohols. When considering its optical properties, pentanol is generally transparent in the visible spectrum. Like other alcohols, pentanol should be handled with care due to its flammable nature and potential health effects. Proper storage and precautions are necessary when working with or around this compound.
Other names and variations
- (C5H8O2)n
- Poly(methyl methacrylate)
- PMMA
- Acrylic glass
- Plexiglas
- Vitroflex
- Limacryl
- R-Cast
- Per-Clax
- Perspex
- Plazcryl
- Acrylex
- Acrylite
- Acrylplast
- Altuglas
- Polycast
- Oroglass
- Lucite
Links