Optical constants of (C5H8O2)n (Poly(methyl methacrylate), PMMA)
Nyakuchena et al. 2023: n 1.10–1.65 µm

Wavelength: µm
 (1.1–1.65)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n=1.4778-5.7547\text{×}10^{-4}λ^{2}+0.0023λ^{-2}$$

Conditions

temperature: 296

Notes

Polymer microspheres. 23 °C

References

M. Nyakuchena, C. Juntunen, P. Shea, Y. Sung. Refractive index dispersion measurement in the short-wave infrared range using synthetic phase microscopy. Phys. Chem. Chem. Phys. 25, 23141-23149 (2023)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Poly(methyl methacrylate)

Pentanol (Amyl alcohol, C5H12O) is an organic compound that belongs to the alcohol family. There are several isomers of pentanol, with the common name "amyl alcohol" often referring to a mixture of these isomers. Predominantly, it's used as a solvent and an intermediate in the production of other chemicals. In its pure form, pentanol has a characteristic alcoholic odor and is slightly viscous compared to lower alcohols. When considering its optical properties, pentanol is generally transparent in the visible spectrum. Like other alcohols, pentanol should be handled with care due to its flammable nature and potential health effects. Proper storage and precautions are necessary when working with or around this compound.

Other names and variations

  • (C5H8O2)n
  • Poly(methyl methacrylate)
  • PMMA
  • Acrylic glass
  • Plexiglas
  • Vitroflex
  • Limacryl
  • R-Cast
  • Per-Clax
  • Perspex
  • Plazcryl
  • Acrylex
  • Acrylite
  • Acrylplast
  • Altuglas
  • Polycast
  • Oroglass
  • Lucite

Links