RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of Montmorillonite
Querry 1987: n,k 2.5–200 µm

Wavelength: µm
 (2.5000–200.0000)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Pellet.

References

M. R. Querry. Optical constants of minerals and other materials from the millimeter to the ultraviolet, Contractor Report CRDEC-CR-88009 (1987)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Montmorillonite

Chemical formula: (Na,Ca)0.33(Al,Mg)2(Si4O10)(OH)2·nH2O

Links