Optical constants of Micro resist ma-N 1407
Sarkar et al. 2019: n,k 0.301–1.69 µm
Wavelength:
µm
(0.3014–1.6880)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions
film_thickness: 1.0E-6 substrate: glass
Notes
Negative tone resist (ma-N 1407) thin film (thickness 1000 nm) on glass substrate.
References
S. Joseph, S. Sarkar, J. Joseph. Grating-coupled surface plasmon-polariton sensing at a flat metal–analyte interface in a hybrid-configuration. ACS Appl. Mater. Interfaces, 12, 46519-46529 (2020) (Numerical data kindly provided by Prof. Joby Joseph)
Data
Additional information
About Resists
In semiconductor fabrication, a resist is a thin layer used to transfer a circuit pattern to the semiconductor substrate which it is deposited upon. (from Wikipedia)