Optical constants of Micro resist EpoClad
Spec sheet: n 0.45–1.55 µm
Wavelength:
µm
(0.45–1.55)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n=1.560+0.0073λ^{-2}+0.00038λ^{-4}$$Notes
Micro resist EpoClad negative photoresist for waveguide manufacturing
References
Data
Additional information
About Resists
In semiconductor fabrication, a resist is a thin layer used to transfer a circuit pattern to the semiconductor substrate which it is deposited upon. (from Wikipedia)
Links