Optical constants of CH3OH (Methanol)
Moutzouris et al. 2013: n 0.450–1.55 µm

Wavelength: µm
 (0.45–1.551)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula

$$n^2=1.745946239-0.005362181λ^{2}+0.004656355λ^{-2}+0.00044714λ^{-4}-0.000015087λ^{-6}$$

Conditions

temperature: 300

Comments

300 K (27 °C).

References

K. Moutzouris, M. Papamichael, S. C. Betsis, I. Stavrakas, G. Hloupis D. Triantis. Refractive, dispersive and thermo-optic properties of twelve organic solvents in the visible and near-infrared. Appl. Phys. B 116, 617-622 (2013)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Methanol

Methanol (CH4O), also known as wood alcohol, is a clear, colorless liquid with a slightly sweet odor. It is the simplest alcohol and is used as an antifreeze, solvent, fuel, and as a feedstock for producing various chemicals. Methanol is flammable and is toxic when ingested, inhaled, or absorbed through the skin. It can cause blindness if ingested. In the field of optics, methanol is often utilized as a solvent in various spectroscopic studies due to its ability to dissolve a wide range of organic compounds.

Chemical formula: CH3OH or MeOH

Other names and variations

  • CH4O
  • Hydroxymethane
  • Methyl alcohol
  • Methyl hydrate
  • Methyl hydroxide
  • Methylic alcohol
  • Methylol
  • Wood alcohol

Links