Optical constants of Metamaterials
Valentine et al. 2008: Metamaterial; n 1.200–1.775 µm

Wavelength: µm
 (1.200–1.775)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

References

J. Valentine, S. Zhang, T. Zentgraf, E. Ulin-Avila, D. A. Genov, G. Bartal, X. Zhang. Three-dimensional optical metamaterial with a negative refractive index. Nature 455, 376-379 (2008) (Data points extracted from a figure)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Metamaterials

Metamaterials are artificial materials engineered to have properties that may not be found in nature. The greatest potential of metamaterials is the possibility to create a structure with a negative refractive index, since this property is not found in any non-synthetic material.