Optical constants of Air
Ciddor 1996: n 0.23–1.690 µm

Wavelength: µm
 (0.23–1.69)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula

$$n-1=\frac{0.05792105}{238.0185-λ^{-2}}+\frac{0.00167917}{57.362-λ^{-2}}$$

Conditions

temperature: 288.15
pressure: 101325

Notes

Standard air: dry air at 15 °C, 101.325 kPa and with 450 ppm CO2 content.

References

P. E. Ciddor. Refractive index of air: new equations for the visible and near infrared. Appl. Optics 35, 1566-1573 (1996)
[Calculation script (Python) - can be used to calculate the refractive index of air for specific values of humidity, temperature, pressure, and CO2 concentration]

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Air

Air is a mixture of gases that constitutes the Earth's atmosphere and is vital for most forms of life on our planet. It primarily consists of nitrogen (approximately 78%) and oxygen (about 21%), with small amounts of other gases such as argon, carbon dioxide, neon, helium, and methane. The exact composition can vary depending on location and environmental conditions. Air is colorless, odorless, and tasteless. From a physical perspective, air plays a crucial role in many processes such as weather patterns, the water cycle, and is also an important medium for sound transmission. In terms of its optical properties, air has a refractive index very close to 1 (approximately 1.0003 at sea level under standard conditions), which varies slightly with temperature, humidity, and pressure. This refractive index is crucial in various applications ranging from astronomical observations to the design of optical systems where light travels through the atmosphere. Understanding the properties of air, including its refractive index, is essential for disciplines such as meteorology, environmental science, aviation, and optical engineering.