Optical constants of Franckeite
Gant et al. 2017: n,k 0.444–0.778 µm
Wavelength:
µm
(0.4439741–0.7776007)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions
substrate: SiO2/Si
Notes
Optical constants derived from reflectance spectra of 25-170 nm franckeite films on SiO2/Si substrate.
References
P. Gant, F. Ghasemi, D. Maeso, C. Munuera, E. López-Elvira, R. Frisenda, D. Pérez De Lara, G. Rubio-Bollinger, M. Garcia-Hernandez, A. Castellanos-Gomez. Optical contrast and refractive index of natural van der Waals heterostructure nanosheets of franckeite. Beilstein J. Nanotechnol. 8, 2357-2362 (2017) (Numerical data kindly provided by Andres Castellanos-Gomez)
Data
Additional information
About Franckeite
Chemical formula: Pb5Sn3Sb2S14
Links