Optical constants of C2H4(OH)2 (Ethylene glycol)
El-Kashef 2000: n 0.4–0.8 µm

Wavelength: µm
 (0.4–0.8)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n=1.386820+17856.021\text{×}10^{-6}λ^{-2}$$

Conditions

temperature: 293

Notes

20 °C

References

H. El-Kashef. The necessary requirements imposed on polar dielectric laser dye solvents. Physica B 279, 295-301 (2000)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Ethylene

Ethylene (C2H4) is a colorless, flammable gas with a slightly sweet odor. It is the simplest alkene and is produced in vast quantities in the petrochemical industry. Ethylene plays a critical role in the synthetic polymer industry, being the precursor to polyethylene, the world's most widely used plastic. Besides its significance in polymer synthesis, ethylene is a naturally occurring plant hormone responsible for fruit ripening and flower wilting. Due to its importance in both industrial and natural processes, ethylene production and its role in plant biology have been extensively studied. In the industrial setting, it's crucial to store and transport ethylene under controlled conditions due to its flammability.

Other names and variations

  • C2H4

Links