Optical constants of C9H10O3 (Ethyl salicylate)
Rheims et al. 1997: n 0.589–1.05 µm

Wavelength: µm
 (0.5893–1.05)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n=1.49376+0.00873λ^{-2}+0.00018λ^{-4}$$

Conditions

temperature: 293

Comments

20 °C

References

J. Rheims, J Köser, T Wriedt. Refractive-index measurements in the near-IR using an Abbe refractometer. Meas. Sci. Technol. 8, 601-605 (1997)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Ethyl salicylate

Ethyl salicylate (C9H10O3) is a clear liquid that emits a faintly sweet, wintergreen-like aroma. It is frequently employed in the flavor and fragrance industry due to its pleasant, minty scent and taste. Apart from its applications in perfumes and as a flavoring agent in certain candies and pharmaceutical products, ethyl salicylate is also utilized in sunscreens and other cosmetic products. Furthermore, this compound has been studied for its potential anti-inflammatory and analgesic properties, making it of interest in medical research.