Optical constants of C4H8O2 (Ethyl acetate, EtOAc, EA)
Kozma et al. 2005: n 0.248–0.641 µm
Complex refractive index (n+ik)
Derived optical constants
Dispersion formula
$$n=1.3662+3.3477\text{×}10^{-3}λ^{-2}-1.3323046\text{×}10^{-5}λ^{-4}+2.87492\text{×}10^{-6}λ^{-6}$$Conditions
temperature: 295
Notes
22 °C
References
I. Z. Kozma, P. Krok, E. Riedle. Direct measurement of the group-velocity mismatch and derivation of the refractive-index dispersion for a variety of solvents in the ultraviolet. J. Opt. Soc. Am. B 22, 1479-1485 (2005)
Data
Additional information
About Ethyl acetate
Ethyl acetate (C4H8O2, EtOAc, EA) is a colorless, volatile liquid with a sweet, fruity odor reminiscent of pear drops. As a medium-polarity solvent, it finds use in a variety of industries, especially in the manufacture of inks, adhesives, and coatings. It's frequently employed as a solvent for extractions in laboratory procedures and in the production of varnishes and nail polish removers. Additionally, due to its pleasant smell, ethyl acetate is occasionally used in the formulation of perfumes and as a flavoring agent in food products.
Chemical formula: CH3-COO-CH2-CH3