Optical constants of C2H5OH (Ethanol)
Chang et al. 2024: n 0.4–2.0 µm

Wavelength: µm
 (0.4–2)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{0.8312λ^2}{λ^2-0.0964^2}+\frac{0.0192λ^2}{λ^2-2.97^2}$$

Conditions

temperature: 295

Notes

21.5–22.0 °C

References

H.-J. Chang, N. Munera, C. Lopez-Zelaya, D. Banerjee, G. Beadie, E. W. Van Stryland, D. J. Hagan. Refractive index measurements of liquids from 0.5 to 2 µm using Rayleigh interferometry. Opt. Mater. Express 14, 1253–1267 (2024)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Ethanol

Ethanol (C2H6O), often simply referred to as alcohol, is a clear, colorless liquid with a characteristic pleasant odor. It is best known as the active ingredient in alcoholic beverages but also has significant industrial and medicinal applications. As a solvent, it is widely used in the pharmaceutical and cosmetic industries. In the medical field, it serves as an antiseptic, disinfectant, and as an antidote in methanol and ethylene glycol poisoning. Ethanol is also used as a renewable fuel and fuel additive, typically referred to as bioethanol, which is produced through the fermentation of sugars by yeast.

Chemical formula: C2H5OH

Other names and variations

  • C2H6O
  • Ethyl alcohol
  • Grain alcohol
  • Pure alcohol
  • Hydroxyethane
  • Drinking alcohol
  • Ethyl hydrate

Links