Optical constants of C7H14O2 (Enanthic acid)
Rubio et al. 2015: n 0.400–0.590 µm

Wavelength: µm
 (0.4–0.59)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n=1.41155+3.92342\text{×}10^{-3}λ^{-2}$$

Conditions

temperature: 293

Notes

20 °C (293 K). For the temperature-dependent formula, refer to the original publication.

References

J. E. F. Rubio, J. M. Arsuaga, M. Taravillo, M. Cáceres. Refractive index temperature and wavelength dependencies of normal saturated fatty acids in liquid state. Exp. Therm. Fluid Sci. 29, 681-684 (2015)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Enanthic acid

Enanthic acid is a saturated fatty acid with a seven-carbon chain. It is a colorless oily liquid with an unpleasant, rancid odor. Naturally occurring in some plant oils, it is used in the synthesis of esters for fragrances and flavors. Industrially, enanthic acid serves as an intermediate in the production of lubricants and plasticizers.

Chemical formula: CH3(CH2)5COOH

Other names and variations

  • C7H14O2
  • Heptanoic acid
  • n-Heptanoic acid
  • Oenanthic acid
  • Enanthylic acid
  • Heptylic acid

Links