Optical constants of C8H11N (Dimethylaniline, DMA)
Li et al. 2022: n 0.321–1.7 µm

Wavelength: µm
 (0.321–1.7)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n=1.5184+1.395\text{×}10^{-02}λ^{-2}-1.710\text{×}10^{-03}λ^{-4}+2.232\text{×}10^{-04}λ^{-6}$$

Notes

Room temperature.

References

X. Li, C. Wang, L. Ma, L. Liu. Ellipsometry-transmission measurement of the complex refractive indices for a series of organic solvents in the 200–1700 nm spectral range. Infrared Phys. Technol. 125, 104313 (2022)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About N,N-Dimethylaniline

N,N-Dimethylaniline (C8H11N, DMA) is an aromatic amine consisting of a benzene ring substituted with a dimethylamino group. It is a colorless to pale yellow oily liquid with a characteristic amine-like odor, which darkens upon exposure to air and light. Dimethylaniline is widely used as an intermediate in the production of dyes, antioxidants, and photographic chemicals. It also serves as a solvent and a reagent in organic synthesis. Due to its toxic and potentially carcinogenic properties, it should be handled with care in well-ventilated environments.

Chemical formula: C6H5N(CH3)2

Other names and variations

  • C8H11N
  • DMA
  • Dimethylaniline
  • N-Methylaniline, N-methyl-
  • N,N-Dimethylbenzenamine
  • Benzenamine, N,N-dimethyl-
  • Aniline, dimethyl-
  • Dimethylphenylamine

Links