Optical constants of C2H6OS (Dimethyl sulfoxide, DMSO)
Li et al. 2022: n 0.2–1.7 µm
Complex refractive index (n+ik)
Derived optical constants
Dispersion formula
$$n=1.4575+8.036\text{×}10^{-03}λ^{-2}-1.581\text{×}10^{-04}λ^{-4}+1.653\text{×}10^{-05}λ^{-6}$$Notes
Room temperature.
References
X. Li, C. Wang, L. Ma, L. Liu. Ellipsometry-transmission measurement of the complex refractive indices for a series of organic solvents in the 200–1700 nm spectral range. Infrared Phys. Technol. 125, 104313 (2022)
Data
Additional information
About Dimethyl sulfoxide
Dimethyl sulfoxide (C2H6OS, DMSO, Me2SO) is a highly polar organic solvent with a wide range of applications. It is a clear, colorless liquid that is miscible with many organic solvents and water. Due to its ability to penetrate biological membranes, DMSO is frequently used as a solvent in biological studies and as a carrier for drug delivery. It also has anti-inflammatory properties and has been used in various medical applications, such as a treatment for pain and inflammation associated with certain conditions. In the industrial sector, DMSO is used as a solvent in chemical reactions, and in the electronics industry, it serves as a photoresist stripper and cleaner.
Chemical formula: (CH3)2SO
Other names and variations
- C2H6OS (DMSO, Me2SO)
- Methyl sulfoxide
- Methylsulfinylmethane
- Sulfinylbismethane
Links