RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of C3H9O3P (Dimethyl methylphosphonate, DMMP)
Querry 1987: Near-infrared; n,k 0.80–2.5 µm

Wavelength: µm
 (0.8045–2.4995)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

References

M. R. Querry. Optical constants of minerals and other materials from the millimeter to the ultraviolet. Contractor Report CRDEC-CR-88009 (1987)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Dimethyl methylphosphonate

Dimethyl methylphosphonate (C3H9O3P) is an organic compound that is commonly used as a flame retardant and as a plasticizer. It is a clear, colorless liquid at room temperature and is soluble in many organic solvents. This compound is characterized by the presence of phosphorus in its molecular structure. In addition to its industrial uses, dimethyl methylphosphonate is often employed as a simulant in studies related to the detection and decontamination of nerve agent threats due to its structural similarities with certain nerve agents.

Other names and variations

  • C3H9O3P
  • DMMP
  • Methylphosphonic acid dimethyl ester
  • dimethoxymethyl phosphine oxide
  • Dimethyl methanephosphonate
  • Dimethyl methyl phosphonate
  • Fran TF 2000
  • Fyron DMMP
  • Metaran
  • NSC 62240
  • O,O-dimethyl methylphosphonate
  • Reoflam DMMP

Links