Optical constants of Diesel soot
Querry 1987: Sample 1, heated; n,k 0.260–55.6 µm
Wavelength:
µm
(0.2600–55.5556)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Notes
Diesel soot sample obtained at New Mexico State University by open burning of diesel fuel. Sample heated to to about 320 °C for about one-half hour to drive off any unburned hydrocarbons.
References
M. R. Querry. Optical constants of minerals and other materials from the millimeter to the ultraviolet, Contractor Report CRDEC-CR-88009 (1987)