Optical constants of Diesel soot
Querry 1987: Sample 1; n,k 0.260–55.6 µm
Wavelength:
µm
(0.2600–55.5556)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Notes
Diesel soot sample obtained at New Mexico State University by open burning of diesel fuel.
References
M. R. Querry. Optical constants of minerals and other materials from the millimeter to the ultraviolet, Contractor Report CRDEC-CR-88009 (1987)