RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of C6H12 (Cyclohexane)
Kozma et al. 2005: n 0.230–0.641 µm

Wavelength: µm
 (0.23–0.6407)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{0.98901λ^2}{λ^2-0.01023416369}+\frac{0.01121λ^2}{λ^2-0.03623317709}$$

Conditions

temperature: 295

Notes

22 °C

References

I. Z. Kozma, P. Krok, E. Riedle. Direct measurement of the group-velocity mismatch and derivation of the refractive-index dispersion for a variety of solvents in the ultraviolet. J. Opt. Soc. Am. B 22, 1479-1485 (2005)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Hexane

Hexane (C6H14) is an alkane hydrocarbon with a straight chain of six carbon atoms. It appears as a colorless liquid that has a mild, gasoline-like odor. Volatile and highly flammable, hexane is often utilized as a solvent in laboratories due to its capability to dissolve non-polar substances. In the industrial realm, hexane is frequently used in the extraction of vegetable oils from crops such as soybeans. Its low polarity makes it ineffective for dissolving polar compounds but efficient for non-polar molecules. In optics, hexane can serve as a medium in certain experimental setups, benefiting from its defined refractive properties.

Other names and variations

  • C6H14

Links