Optical constants of Colon
Giannios et al. 2017: Mucosa; n,k 0.45–1.551 µm

Wavelength: µm
 (0.45–1.551)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n=1.321743411+0.009941336λ^{-2}-0.000890957λ^{-4}$$

Notes

24 °C ± 2 °C.

References

P. Giannios, S. Koutsoumpos, K. G. Toutouzas, M. Matiatou, G. C. Zografos, K. Moutzouris. Complex refractive index of normal and malignant human colorectal tissue in the visible and near-infrared. J. Biophotonics 10, 303-310 (2017)