Optical constants of Blood
Liu et al. 2019: Serum; n 0.400–0.750 µm

Wavelength: µm
 (0.4–0.75)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n=1.3350+4.6513\text{×}10^{-3}λ^{-2}-1.3069\text{×}10^{-4}λ^{-4}$$

References

S. Liu, Z. Deng, J. Li, J. Wang, N. Huang, R. Cui, Q. Zhang, J. Mei, W. Zhou, C. Zhang, Q. Ye, J. Tian. Measurement of the refractive index of whole blood and its components for a continuous spectral region. J. Biomed. Opt. 24, 035003 (2019)